To eliminate the change of hardness from super
heat generated in friction welding and to get the
proper high strength in coupling, ASAN takes high
tensile strength over 100§¸·f/§±
through quenching & tempering by HRc 30.
Also, after Q/T treatment thread part both pin
and box to be induction hardened at HRC 50
hardness.
[Heat Treatment]
¡¡
¡¡